Abstract

Research on concrete which is ongoing at this time aims to obtain good quality and high quality concrete, to get it it needs to be mixed with additives (Admixture) as an added material for concrete mixtures. Sika Viscocrete is an added material that can help concrete improve its performance at a faster time and has the dual function of reducing the amount of water mixing required to produce concrete with a certain consistency and speed up the bonding of the concrete. The purpose of this study was to determine the effect of adding the additive ViscoCrete sika to the compressive strength of the K-300 concrete. The sample used was 15cm x 15cm x 15cm cuboid at the age of 14 days. With variations, namely Normal Concrete and Normal Concrete + Sika Viscocrete 1%, 2%, 3% with 9 samples in each variation. The results showed that the value of the compressive strength of concrete with the addition of 2% Sika Viscocrete-3115N aged 14 days to normal concrete was 315, 07 Kg / Cm2. While the addition of 3% Sika Viscocrete-3115N obtained the optimum value at the age of 14 days of 358.13 Kg / Cm2.

 

Kata Kunci : K-300 Concrete, Additives, Viscocrete Sika and Concrete Presure

Author Biographies

R.R. Susi Riwayati, Universitas Tamansiswa Palembang

Program Studi Teknik Sipil Fakultas Teknik 

Roby Habibi, Universitas Tamansiswa Palembang

Program Studi Teknik Sipil Fakultas Teknik 

References

Abas, Syazili.2014. Concrete technology. Jakarta

Agustian, Muhammad Robin. 2018. Pengaruh Penambahan Aditif Bestmittel

dan Pengurangan Air Terhadap Kuat Tekan Beton K-300. Universitas Muhammadyah Palembang.

Pascal, Dimas Septio. 2019. Pengaruh Pemakaian Superplasticizer (Sika Viscocrete) Pada Kuat Tekan Beton Mutu Tinggi K-500. Universitas Muhammadyah Palembang.

Idn.sika.com

https://lawtjunnji.weebly.com/curing-beton.html

Astuti. 2006. Susunan Unsur Semen OPC

Aji, Pujo, dan Purwono, Rachmat. 2010. Pengendalian Mutu Beton. Surabaya.

Mulyono, Tri. 2003. Teknologi Beton. Yogyakarta.

Mulyono, Tri. 2004. Teknologi Beton. Yogyakarta.

Mulyono, Tri. 2005. Teknologi Beton. Yogyakarta.

Nugraha, Paul dan Antoni. 2007. Teknologi Beton. Yogyakarta.

SNI-2847-2013, Persyaratan Beton Struktural Untuk Bangunan Gedung. Jakarta

SNI S-04-1989-F, Spesifikasi Bahan Bangunan A/Bahan Bangunan Bukan Logam

SNI-03-1968-1990, Metode Pengujian Tentang Analisis Saringan Agregat Halus dan Kasar

SNI-T-15-1991-03, Tata Cara Perhitungan Struktur Beton Untuk Bangunan Gedung. Bandung.

SNI-T-03-2834-1993, Tata Cara Campuran Beton Normal. Jogja

SNI-03-6815-2002, Tata Cara Mengevaluasi Hasil Uji Kekuatan Beton. Jakarta

Tjokrodimuljo, Kardiyono. 1992. Teknologi Beton. Yogyakarta.

Tjokrodimuljo, Kardiyono. 1996. Teknologi Beton. Yogyakarta.

Tjokrodimuljo. 2007. Teknologi Beton. Yogyakarta.

Newman dalam Murdock (1999) Murdock, L. J. Dan Brook, K. M., Bahan dan Praktek Beton; diterjemahkan oleh Ir. Stephanus Hendarko, Jakarta: Erlanggan.

Downloads

Published

2021-02-05

How to Cite

Riwayati, R. S., & Habibi, R. (2021). Pengaruh Penambahan Zat Aditif Sika Viscocrete Terhadap Kuat Tekan Mutu Beton K-300 Umur 14 Hari. Jurnal Tekno Global, 9(2). https://doi.org/10.36982/jtg.v9i2.1293

Issue

Section

Articles